    Swift Trawler 35 Fiberglass/Gel coat cracking

    Photos Im new to this forum, so hopefully i didn't make a mess and upload them 10 times. Boat has never been in any collisions and has been in calm inland water its entire life.
  2. D

    Swift Trawler 35 Fiberglass/Gel coat cracking

    sorry about the delay in posting the pictures. Theres two photos of each, one to give location and one closeup. This isn't an exhaustive list, just the main ones. The hull has a 7 year warranty from manufacturer (Beneteau), of which two years remain. Current plan is to have it professionally...
  3. IMG 5172

    IMG 5172

  4. IMG 5171

    IMG 5171

  5. IMG 5169

    IMG 5169

  6. IMG 5170

    IMG 5170

  7. IMG 5168

    IMG 5168

  8. IMG 5166

    IMG 5166

  9. IMG 5167

    IMG 5167

  10. IMG 5165

    IMG 5165

  11. 2018 ST 35 hull cracks

    2018 ST 35 hull cracks

    presumed stressed induced gel coat cracks, currently working to resolve.
  12. D

    Swift Trawler 35 Fiberglass/Gel coat cracking

    I have a 2018 ST 35 that is cracking at areas of geometric inflection.....i.e. inside of corners etc. Is this common? Anybody else have similar experience? Its going back to the dealer for some other work in a few months, trying to figure out my approach. I'll take and posts pics asap.