Pack Mule
TF Site Team
- Joined
- Jan 24, 2013
- Messages
- 3,749
- Location
- USA
- Vessel Name
- Slo-Poke
- Vessel Make
- Jorgensen custom 44
Ok we repainted our aft deck this past spring . We used 1 prt poly Interlux . We cleaned it and primed it first . Then put on two coats paint . Last coat I added some color flakes to help hide some defects . Now I'm thinking we should have used two part paint . This stuff doesn't seem like it dried all the way . After sitting in deck chairs and moving back and forth its peeling paint up . I guess I laid the paint on too heavy and it dried on top and not underneath . This is not pretty .
What is going to be our best method of fixing this ? It's not going to strip very well because of nonskid .
What is going to be our best method of fixing this ? It's not going to strip very well because of nonskid .